A silo that discharges perfectly on Monday can block on Wednesday with the same product. Usually the material has changed — moisture, particle size distribution, or simply how long it sat there.
1. Get the cone angle right
Free-flowing granules may run out of a 45° cone; fine cohesive powder often needs 60–70°, and some products need a mass-flow design where the whole bed moves rather than a funnel down the middle. If the angle is wrong, no vibrator will fix it permanently.
2. Break the arch, do not shake the silo
Air cannons and fluidising pads inject energy where the arch forms. A pneumatic vibrator on the cone is cheaper, but on a large silo it mostly makes noise. For cohesive powder, an aeration pad that creates a thin air film at the wall is often the most effective option.
3. Keep the outlet moving
A rotary valve or a properly sized butterfly valve that opens fully prevents the material from consolidating in the outlet. Partially open valves are a common cause of rat-holing.
4. Design the finish
Rough welds and internal ledges give powder somewhere to hang. A polished internal surface (Ra ≤ 0.2 μm) with radiused corners and no crevices removes the starting point for most arches.
Send us the angle of repose and the moisture content of your product, and we will specify the cone and the flow aid together rather than adding a vibrator after the first blockage.
Equipment used for this duty
Machines from our catalogue that solve the problem described above.
- Big-Bag Unloader — Sealed FIBC discharge cabinet with dust extraction and flow-assist options.
- Dust-Free Dumping Station — Production booth with 1.1–1.5 kW extraction fan and 0.5 μm cartridges — the standard TLZ series.
- Reactor Vacuum Loader — Fully pneumatic loader for charging reactors with solvent-wet or explosive powders, nitrogen blanketing available.
Have a technical question about this topic?
Ask our engineers